Influence Of Carbon On Sox Emissions From Glass Processing

Carbon reacts with Na2SO4 in glass batches, influencing SOx emissions. To study the role of carbon active surface area (ASA) in the decomposition phenomena, Na2SO4 is reacted with three carbons with a wide ASA range.