Inertial Filtration Alternative For Dust Control

European glass manufacturers are having to review their investments in emissions control equipment in order to comply with environmental regulations. This paper looks at inertial separators as viable alternatives for controlling dust.

Author
E Johnson
Origin
Global Filtration Systems, Uk
Journal Title
Glass 77 5 2000 129
Sector
Container glass
Class
C 1548

Request article (free for British Glass members)

Inertial Filtration Alternative For Dust Control
Glass 77 5 2000 129
C 1548