Indonesia's glass industry plays a significant role in the South East Asian glass market. The country has long been accused of dumping its glass products in the region, often painting a grim picture of domestic consumption. Conversely, it has been able to produce finished products at a much lower rate compared to some of its neighbours. The industry includes some well-known names, companies known for the quality of their products, not only in Indonesia but internationally. Its glass tableware industry is counted among the top five countries worldwide. The Indonesian glass container industry has continued to grow at a CGAR of 6% in the past five years. This article takes a look at Indonesia's glass container manufacturing sector, and factors influencing the market.

Author
Un-named
Origin
Unknown
Journal Title
Glass Worldwide July-Aug/2011 80, 82
Sector
Container glass
Class
C 4454

Request article (free for British Glass members)

Indonesian Glass Container Industry Review
Glass Worldwide July-Aug/2011 80, 82
C 4454
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
9 + 4 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.