Indentation Behaviour Of Soda-Lime-Silica Glass, Fused Silica, And Single-Crystal Quartz At Liquid Nitrogen Temperature

In an attempt to elucidate the processes involved in the formation of indentation impressions, Vickers hardness measurements have been made on soda-lime silica glass, fused silica, and crystalline quartz indented at room temperature and 77 K.

Author
C R Kurkjian & G W Kammlott
Origin
At & T Bell Labs, New Jersey, Usa
Journal Title
J Am Ceram Soc 78 3 1995 737-744
Sector
Special Glass
Class
S 852