Increased Glass Block Production Rates

During Milan's Vitrum 2001, German glass manufacturing plant producer J Walter Co., previewed a new twin line for glass block production. This article looks at the innovative concept at the heart of the new line, the importance of Walter's expertise in memory-programmable controls, and servo and hydraulic systems in delivering the increased production rates now possible.