Imrpoving Regenerator Efficiency

A new solution has been implemented in a large end port furnace for container glass. It led to an increase in efficiency with no other impact on furnace working conditions.

Author
D Lechvalier Et Al
Origin
Saint-Gobain Sefpro
Journal Title
Glass International Sept/2012 33-34, 36