Improvements In Ultrasonic Inspection For Fused Cast Refractories

Ultrasonic testing has been a necessary tool for nondestructive characterisation of fused cast refractories. In this paper some further studies are presented involving the testing of sample shrinkage cavities, testing of monolithic shrinkage cavities and the determination of the residual thickness of refractories.