Improvements In Or Relating To The Manufacture Of Flat Glass

A fender which halts the flow of an advancing layer of molten glass in the float process is a hollow channel of a material not wetted by molten glass. A flat face which engages the glass extends downwards into a foot which is immersed in the molten metal of the bath. Fluid to cool the face is passed through a groove in the foot near the face.

Author
G.A. Dickinson And F. Nixon
Origin
Pilkington Brothers Limited
Journal Title
(S.A.P 69/5455, 29.1.71)
Sector
Primary Papers
Class
PP 267

Request article (free for British Glass members)

Improvements In Or Relating To The Manufacture Of Flat Glass
(S.A.P 69/5455, 29.1.71)
PP 267