Improvements In Or Relating To The Flotation Process For Producing Continuous Glass Ribbon

Contaminating gases are removed from the refractory ceramic structure forming thefloat bath by the circulation of a stream of hydrogen through the structure. The molten metal in the bath may be removed from the bath and vacuum degassed to partially remove hydrogen dissolved in the metal.