Improvement Of Glass Surface Strength With Polymeric Coatings (In French)

Manufacturing of coatings is usually performed in order to improve mechanical, tribological or electrochemical properties of materials. For instance, especially in the case of bottles, a polymeric coating enhances the mechanical strength by closing the pre-existing cracks. A better solution is to use a composite coating: polymeric matrix and inorganic reinforcing particles. This paper addresses this problem. Firstly, composition and microstructure of two kinds of bulk composite materials are presented: either a mixture of a polymeric matrix (HEMA) and preformed silica particles (average diameter about 13nm), or a composite developed by in-situ polymerisation of HEMA and a silica precursor. In the second step, composition is optimised for coating, by addition of other polymeric components with specific properties and thermal treatment is carried out.

Author
P Hajji Et Al
Origin
Elf-Atochem, France
Journal Title
Verre 6 2 2000 9-20
Sector
Special Glass
Class
S 1933

Request article (free for British Glass members)

Improvement Of Glass Surface Strength With Polymeric Coatings (In French)
Verre 6 2 2000 9-20
S 1933
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 4 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.