Improvement Of Batch Preparation And Feeding For Glass Furances

The factors affecting the maintenance of stable batch quality when batch is loaded into glass furnaces after being transported from a sectional shop over a long distance are analysed. The deficiencies arising during batch preparation and transport to a glass furnace are analysed. A new method of loading batch into a glass furnace is proposed on the basis of the analysis: this method makes it possible to support optimal moisture content and uniformity of batch prior to loading into the furnace. The new method of loading batch has been tested in a glass furnace at "Salavasteklo" JSC.

Author
V I Litvin Et Al
Origin
Unknown
Journal Title
Glass & Ceramics 68 5-6 Sept/2011 139-142
Sector
General
Class
G 3934a

Request article (free for British Glass members)

Improvement Of Batch Preparation And Feeding For Glass Furances
Glass & Ceramics 68 5-6 Sept/2011 139-142
G 3934a
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
6 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.