Improved Surface Finishing Achieved With Air Bearing Technology

The Geometric Surfacing Machine uses air bearing technology to achieve flat surfaces of extremely accurate geometry and high surface quality on a wide range of materials that would otherwise require multiple processes to achieve the same result.