Important Advances In The Lehr Belt Design And Performance

A brief history of the evolution of the lehr belt, highlighting the major advances in the design and their benefits to the glass industry, is given.

Author
J D Carduff, C Esterson
Origin
Cambridge Wire Cloth Company
Journal Title
Glass Production Technology International 1992 133-136
Sector
General
Class
G 776a