The Importance Of Oxygen Management When Filling

Bottling represents a critical stage in the life cycle of wine, and other products such as beers etc. For this reason, it must be managed with competence and accuracy. MBF, one of the world's leading manufacturers of complete lines for bottling wines and spirits, in conjunction with the Department of Biotechnology at the University of Verona, have developed a pioneering system for the measured control of oxygen.