The Impervious Membrane Seal For Float Glass Plenum Chambers.

Leakage of air into the atmosphere above a molten metal float bath is prevented by wrapping a gas impervious, heat resisting membrane such as metal foil around the flange and covering the opening of the side wall of the plenum chamber over the bath.