Impedance Spectroscopy Applied To Annealing Effects On Glassy Agpo3:Sub Tg Surface Crystallisation And Glass Relaxation

Impedance spectroscopy is used to follow variations of electrical properties during annealing of an AgPO3 glass below Tg. Surface crystallisation is observed and electrical properties of the crystalline and glassy phases are studied with time and temperature. Variations of electrical conductivity with annealing are related to thermodynamic properties due to glass relaxation.

Author
Y Grincourt Et Al
Origin
Lab D'Ionique Et D'Electrochimie Des Solides De Grenoble, France
Journal Title
Phys Chem Glasses 36 3 1995 123-126
Sector
Special Glass
Class
S 870

Request article (free for British Glass members)

Impedance Spectroscopy Applied To Annealing Effects On Glassy Agpo3:Sub Tg Surface Crystallisation And Glass Relaxation
Phys Chem Glasses 36 3 1995 123-126
S 870
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
5 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.