Impact Of Glass Corrosion On Drug Substance Stability

The delamination of glass contact surfaces because of hydrolytic instability has been well documented. However, the lack of glass surface integrity can also lead to other undesirable outcomes prior to visible glass delamination. This work shows how the early stages of delamination, namely, glass corrosion, can influence the chemical stability of active pharmaceutical ingredient (API) solutions contained within a glass container, even prior to the observation of visible delamination. Multiple containers, all constructed of glass classified as USP Type I, were evaluated for hydrolytic stability and how they influence the chemical stability of the API in question. The glass composition of these analytical consumables, the vendor source, and presumably manufacturing process were examined. The implications of glass container durability on product development decisions, the influence on analytical results, and the practice of like-for-like glass container interchangeability are considered.

Author
M A Watkins
Origin
Ely Lilly & Co, Usa
Journal Title
J Pharmaceutical Sciences 103 8 August 2014 2456-2463
Sector
Container glass
Class
C 5619

Request article (free for British Glass members)

Impact Of Glass Corrosion On Drug Substance Stability
J Pharmaceutical Sciences 103 8 August 2014 2456-2463
C 5619
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
6 + 14 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.