Immobilisation Of Radioactive And Non-Radioactive Wastes In Glass- Based Systems: An Overview

Glass-based systems used or proposed for immobilising radioactive wastes are reviewed and compared with systems suggested for immobilising non- radioactive wastes. The experiences gained in the nuclear field, and how these can be put to good advantage in the development of new glass-based systems and facilities for immobilising non-radioactive wastes, are highlighted.

Author
I Donald
Origin
Materials Science Research Division, Awe, Berkshire, Uk
Journal Title
Glass Technology August 2007 Volume 48 4 155-163
Sector
Special Glass
Class
S 3317

Request article (free for British Glass members)

Immobilisation Of Radioactive And Non-Radioactive Wastes In Glass- Based Systems: An Overview
Glass Technology August 2007 Volume 48 4 155-163
S 3317
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.