Illustration Of The Cause Of Flux-Line Attack In Glass-Tanks

Window-glass melted in contact with an aluminous refractory shows meniscus phenomena similar to those seen with alcohol-water mixtures in a wine glass. These phenomena depend on the alkaline content, not the sulphate content, of the glass.

Author
J. Loeffler
Origin
Unknown
Journal Title
Glaastechn. Ber., 41, (12) 513 1968 (German)
Sector
Primary Papers
Class
PP 971

Request article (free for British Glass members)

Illustration Of The Cause Of Flux-Line Attack In Glass-Tanks
Glaastechn. Ber., 41, (12) 513 1968 (German)
PP 971
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
16 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.