Identification Of The Structure Of The Three-Dimensional Flow In An Idling Container Glass Melter

A three-dimensional numerical model was used to determine the extent to which various tank design parameters influence the structure of the thermal flow of the melt; these include heat losses from the walls and bottom, tank depth, and thermal boundary conditions at the free surface.

Author
A Ungan, R Viskanta
Origin
Purdue University
Journal Title
Glass Technology 1987 28 6 252-260
Sector
Container glass
Class
C 20