Hzfc: Developments, Evolutions, Myths And Misunderstandings

When speaking about refractories, we must bear in mind the changes that take place continuously in this highly aggressive environment of glass furnaces. And this means that products used in the furnaces also need to be able to withstand the high speed of glass movement, improved furnace design and the extended life of furnace campaigns. In this article, the author discusses the developments of High Zirconia Fused Cast materials, and how the product might be evolved for the future.

Author
P C Ratto
Origin
Fused Cast Technologies, Italy
Journal Title
Gmpa 2/2015 65-69
Sector
Refractories
Class
R 831