Hyperfine Splitting And Anisotropy Of Magnetite Particles Within A Glass Matrix By Mossbauer Spectroscopy

The Mossbauer spectra of a basalt glass containing about 13 wt% Fe2O3, which forms magnetite on heat-treatment, have been studied both at 300 K and at 4 K and without magnetic field.

Author
A K Bandyopadhyay, P Auric
Origin
Montpellier University, Centre Of Nuclear Studies, Grenoble
Journal Title
Transactions Of The Indian Ceramic Society 1987 46 5 136-141