Hydrogen Reactivity As A Structural Probe For Glasses

This study investigates the feasibility of using the reaction of hydrogen to study the local structure of barium galliosilicate glasses.

Author
C M Shaw, J E Shelby
Origin
Alfred University, New York, Usa
Journal Title
Physics & Chemistry Of Glasses 34 1 1993 35-41
Sector
Special Glass
Class
S 709