Hydrogen-Containing Glass And Gas-Ceramic Microfoams: Raman, Xps, And Mas-Nmr Results On The Structure Of Precursor Sio2-B2O3-P2O5 Glasses

Raman spectroscopy, photoelectron spectroscopy and magic angle spinning nuclear magnetic resonance have been used to analyse the structure of a series of glasses in the silica-boron-phosphorus system which, on heat treatment, develop a cellular microstructure containing hydrogen gas.

Author
J E Dickinson, B H W S De Jong, C M Schramm
Origin
Corning Glass Works, Catalytica Associates
Journal Title
Journal Of Non-Crystalline Solids 1988 102 196-204
Sector
Special Glass
Class
S 238

Request article (free for British Glass members)

Hydrogen-Containing Glass And Gas-Ceramic Microfoams: Raman, Xps, And Mas-Nmr Results On The Structure Of Precursor Sio2-B2O3-P2O5 Glasses
Journal Of Non-Crystalline Solids 1988 102 196-204
S 238
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
16 + 4 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.