How Mathematical Modeling Can Help Reduce Energy Usage For Glass Melting

State-of-the-art techniques of modeling of glass melting furnaces give a time averaged solution of the whole (coupled) model. This method seems to be satisfactory to obtain accurate heat fluxes between the glass and combusiton space, and thus to have a good boundary condition for the glass model to evaluate al the values of interest, such as glass flow patterns, temperatures, batch shape, quality indices, seed counts, and so on. However, in modeling combusiton chambers of regenerative furnaces, we can see processes that, because of their nature, are time-dependent and cannot be represented by a time-averaged steady state. This paper presents results of simulations of two designs of a regenerator. Some drawbacks of traditional regenerator designs are identified and improvements suggested.

Author
E Muijsenberg & M Trochta
Origin
Glass Service Inc, The Netherlands
Journal Title
Cesp 64 Conf Glass Problems 25 1 2004 167-177
Sector
General
Class
G 2822

Request article (free for British Glass members)

How Mathematical Modeling Can Help Reduce Energy Usage For Glass Melting
Cesp 64 Conf Glass Problems 25 1 2004 167-177
G 2822
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.