How Does Glass Form? Mdi Research Team Set To Get Some Answers On The International Space Station

Characterising glass structure is elusive, because it is amorphous and impacted by almost everything: composition; thermal history; dimension; time; etc. Motivated by the need to understand and manipulate glass structure, glass researchers have sought accurate modelling strategies to drive innovation in the glass industry and its search for new compositions and better processes, as described in this article.

Author
Un-named
Origin
Unknown
Journal Title
Am Ceram Soc Bull 95 8 Oct-Nov 2016 16-17
Sector
News Items
Class
N 3678

Request article (free for British Glass members)

How Does Glass Form? Mdi Research Team Set To Get Some Answers On The International Space Station
Am Ceram Soc Bull 95 8 Oct-Nov 2016 16-17
N 3678
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
11 + 8 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.