How Are Superstructure Refractories Meeting Today'S Challenges ?

Factors affecting usage of superstructure refractories in glass melting furnaces are reviewed briefly.

Author
T Busby
Origin
Fosbel Inc
Journal Title
Glass Industry March 1990 31, 35
Sector
Refractories
Class
R 42