Hot Glass - A Cooling Solution At Last

In container manufacture, one of the biggest problems facing production managers is effective and efficient glass conditioning. Modern forehearths are advancing at a rapid pace and are getting ever more efficient at delivering glass at a homogeneous temperature to the orifice. In this article the author presents some innovative solutions to the problem of hot glass passing through the throat and placing an additional burden on the distributor layout.