Hot End Treatment Developed For Glass Bottles

Sepoan 601 TC is designed as a hot end treatment for glass bottles, produced using a base material called tin tetrachloride. Through vigorous industrial investigation by Pedro Segura SL, in cooperation with Murcia University in Spain, it was possible to eliminate the smoking character of this substance, thus realising less chlorides and solid particles in suspension to the atmosphere. Spanish supplier Pedro Segura SL claims that the possible dangers resulting from the formation of toxic gases when its range of products comes into contact with the free atmosphere or through accidental drum breakage is practically non-existent with Sepoan 601 TC.

Author
Un-named
Origin
Unknown
Journal Title
Glass International May 2008 63
Sector
Container glass
Class
C 3681

Request article (free for British Glass members)

Hot End Treatment Developed For Glass Bottles
Glass International May 2008 63
C 3681
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.