Hot End Imaging: The I-Care Solution

MSC decided six years ago, to develop a process-oriented hot-end inspection system to provide glass manufacturers with the tools they need to objectively analyse and optimise the bottle and jar manufacturing process. The result was I-CARE, which marks a substantial step forward in improving the glass container forming process when used consistently with and in conjunction with cold-end inspection systems. This article describes the system, however, more information can be obtained from the website: www.msc.fr or email: [email protected]

Author
G Lecat & B Guestin
Origin
Msc, France
Journal Title
Glass June 2006 18-19
Sector
Container glass
Class
C 3023

Request article (free for British Glass members)

Hot End Imaging: The I-Care Solution
Glass June 2006 18-19
C 3023
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 8 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.