Hot Batch Enhancement

For decades, Zippe Industrieanlagen has focused on batch preparation and cullet handling technology. Despite numerous improvements and innovations in this field over the years, the aim has principally stayed the same, to produce/create batch according to the precise batch formula and transport and charge it reliably in the correct quality and quantity to the doghouse - all with low dust emissions and minimal wear. The technology is synchronised and controlled by modern process automation software, which increases safety, comfort and efficiency. In this article the author discusses the conditions under which batch preheating can be an economic and feasible integral part of batch preparation.

Author
Dr P Zippe
Origin
Zippe, Germany
Journal Title
Glass Worldwide Nov-Dec/2013 76, 78
Sector
General
Class
G 4172

Request article (free for British Glass members)

Hot Batch Enhancement
Glass Worldwide Nov-Dec/2013 76, 78
G 4172
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
7 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.