[History] The World'S First Successful Regenerative Furnace

The world's first commercially successful regenerative furnace was built by Friedrich Siemens for a small glass making company at Rotherham, South Yorkshire, in 1860. Success came after several years of trials and rapidly led to other larger British glass makers to commission such furnaces which soon became widely used. Most accounts of the development of regenerative furnaces by William and Friedrich Siemens ignore the first glass furnace and assume that earlier trials with steel-making in Sheffield were the first to succeed, but those all failed, largely for lack of sufficiently good refractory materials. The important facts were reported in detail by R Ehrenberg in 1906, but his account has been ignored. This article takes a closer examination of the facts.

Author
M Cable
Origin
University Of Sheffield
Journal Title
Glass Technology 54 3 2013 93-99
Sector
General
Class
G 4184

Request article (free for British Glass members)

[History] The World'S First Successful Regenerative Furnace
Glass Technology 54 3 2013 93-99
G 4184
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
11 + 5 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.