Hindustan Expand Container Capacity

Hindustan Sanitaryware & Industries Ltd recently announced that it plans to invest INR 2.1BN to expand its container glass capacity. The expansion in capacity will be carried out at a greenfield site in Andhra Pradesh state, the company said in a statement.