High Zirconia Fused-Cast Refractories: A Solution To Defect And Corrosion Problems In Special Glasses

Basically, special glasses can be divided into five families: borosilicate glasses; opal glasses; potassium glasses; glass ceramics; and, glasses for reinforcing fibres. The high quality of products manufactured using these types of glass is such that the behaviour of the refractories they are in contact with is extremely important. In fact, the maximum level of glass defects which can be accepted dictate the choice of refractory products used in the furnaces. This article considers possible solutions to these problems and describes the principle defects found in special glasses.

Author
A Zanoli Et Al
Origin
Sepr, France
Journal Title
Fundamentals Of The Glass Manufacturing Process 1991. Esg Conf. 234-238
Sector
Special Glass
Class
S 781

Request article (free for British Glass members)

High Zirconia Fused-Cast Refractories: A Solution To Defect And Corrosion Problems In Special Glasses
Fundamentals Of The Glass Manufacturing Process 1991. Esg Conf. 234-238
S 781
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
20 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.