High-Temperature Uv-Vis-Nir Spectroscopy Of Chromium-Doped Glasses

Chromium-doped glasses with the basic composition (in mol%) 16 Na20.10 CaO.74 Si02 were melted under different redox conditions. From these glasses, UV-VIS-NIR absorption spectra were recorded at temperatures up to 1200 deg C.

Author
D Godeke Et Al
Origin
Otto-Schott-Inst, Jena
Journal Title
Glastech Ber Glass Sci Technol 74 6 2001 177-182
Sector
Special Glass
Class
S 2219

Request article (free for British Glass members)

High-Temperature Uv-Vis-Nir Spectroscopy Of Chromium-Doped Glasses
Glastech Ber Glass Sci Technol 74 6 2001 177-182