High Temperature Superconductivity

Although the technology of high temperature superconductors is only about six years old, progress has been extraordinarily rapid with several commercial applications already available.

Author
N Alford
Origin
Ici Superconductors
Journal Title
Ceramic Technology International 1994 89-92
Sector
Glass Ceramics
Class
GC 143