High-Temperature Spectroscopic Study Of Redox Reactions In Iron And Arsenic-Doped Melts

Glasses with the basic composition 16Na20.10Ca0.74Si02 doped with iron and arsenic were studied by means of high temperature UV-VIS-NIR spectroscopy.