High-Temperature Rheology Of Calcium Aluminosilicate (Anorthite) Glass-Ceramics Under Unaxial And Triaxial Loading

The high-temperature creep behaviour of two fine-grained anorthite-rich glass ceramics was characterized at ambient pressure and under a confining pressure of ~300MPa.