High Temperature Raman Spectra Of Rapidly Quenched 50Li4Sio4, 50Li2Wo4 Glass

High temperature Raman spectra of this rapidly quenched glass, composed of two lithium ortho oxysalts, are measured at various temperatures.

Author
M Takahashi Et Al
Origin
Osaka Municipal Tech Res Inst, Uni Osaka Prefecture, Japan
Journal Title
Phys & Chem Glasses 1992 33 1 9-11
Sector
Special Glass