High-Temperature-Infrared Spectra Of Nioboborate Glass Melts

The structure of nioboborate glass melts in the system has been studied for the first time by high-temperature IR spectra. The structure models of the glass melts and the glasses have been established.

Author
Y Quanzu Et Al, L Donghui
Origin
Changchun Inst Of Optics And Fine Mechanics, China
Journal Title
Glastechnische Berichte 1991 64 9 229 - 234
Sector
Special Glass
Class
S 590

Request article (free for British Glass members)

High-Temperature-Infrared Spectra Of Nioboborate Glass Melts
Glastechnische Berichte 1991 64 9 229 - 234
S 590