High Temperature Corrosion Testing Of Glass Lined Steel

Smith Corporation produces chemical storage vessels & water heaters. Single & multiple coats of enamels are applied to metal substrates, typically hot rolled or cold rolled steels. The glass coating on steel & porcelain enamels are produced & applied in-house. Qualification testing concerning maximum operating temperature, chemical concentration of solutions in contact with glass & the subsequent corrosion rate is of great importance. Corrosion testing methodology has been developed to obtain corrosion rate data for glasses & then extrapolating this data for service life. A high pressure test cell was designed allowing exposure of only the enamel coating to the corrosive liquid. Key factors affecting glass performance coatings are: concentration of the liquid in contact with the glass, temperature of the liquid, the rate of agitation & any contaminants.

Author
G Griffith
Origin
Ao Smith Corporation
Journal Title
67Th Porcelain Enamel Technical Forum 2005 61-68
Sector
General
Class
G 3111

Request article (free for British Glass members)

High Temperature Corrosion Testing Of Glass Lined Steel
67Th Porcelain Enamel Technical Forum 2005 61-68
G 3111
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 12 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.