High-Strength, Large-Case-Depth Chemically Strengthened Lithium Aluminosilicate Glass

High-glass-transition-temperature lithium aluminosilicate glass was chemically strengthened by immersion in NaNO3+KNO3 salt baths for applications requiring a high resistance to fracture upon flexing from projectile impact.

Author
A K Varshneya & I M Spinelli
Origin
Unknown
Journal Title
Am Ceram Soc Bull 88 5 2009 27-33