High-Speed Polymer Optical Fiber For Multimedia Network (In Japanese)

High-bandwidth Graded-Index Polymer Optical Fibre (GI-POF) can be used as a high density information transmission medium maintaining a large core diameter (about 1mm). In this study a low-loss and high-bandwidth GI-POF has been developed. Excellent transparency in the near infrared region could be achieved by using all-fluorinated polymer. Moreover, the GI-POF which has the bandwidth of 2 GHz in the 100m length was successfully prepared by controlling the refractive index distribution of the core area appropriately using this polymer. (abstract only)

Author
Y Koike
Origin
Keio University, Japan
Journal Title
Reports Of Research Asahi Glass Foundation 1997 1-2
Sector
Glass Fibre
Class
GF 186

Request article (free for British Glass members)

High-Speed Polymer Optical Fiber For Multimedia Network (In Japanese)
Reports Of Research Asahi Glass Foundation 1997 1-2
GF 186
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.