High Speed Hot End Coating For Hollow Glass

GlassChem's HECSt 1800 hot end coating system for high speed bottle production lines was introduced at the end of 2011. Subsequently, this equipment has been successfully brought into operation on a glass container production line working at speeds of around 600/bpm. This article describes the latest coating innovation, and the system's success on high speed lines.