High Resolution Laser Inspection Of Glass Plates

Manufacturers of high quality glass plates (eg coated or display glass) are experiencing mounting pressure to boost production rates, improve quality and increase yields. This trend is further stimulated by a continuously increasing size of the glass substrates. Automatic inspection systems can cope with these requirements concurrently if the correct inspection system is installed. The difficulty is matching the inspection problem against an array of inspection system solutions. This article emphasises the inspection of high-quality glass plates. However, the same principles and concepts can be extended to any coated glass application where quality is vital. On the basis of SIS systems in the field, a typical application is described as well as some of its underlying principles.

Author
Dr H Schwarz
Origin
Sis Surface Inspection Systems
Journal Title
Glass Coatings 1/2005 30-31
Sector
Flat glass
Class
F 1756

Request article (free for British Glass members)

High Resolution Laser Inspection Of Glass Plates
Glass Coatings 1/2005 30-31
F 1756
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.