High Refractive Index Optical Glasses Containing Geo2

Covers glasses of RI 1.80-1.96 and Abbe value 32-43 having compositions (Wt%) 20-50 GeO2, 30-50 La2O3, 0-15 BaO, 0-10 B2O3, 0-30 Ta2O5, and 0.30 Nb2O3, preferably 20-32, 35-43, 10-15, 0-6, 15-20, 0, in the same order, with, in addition, oxides of at least one of Li, Na, K, Mg, Ca, Sr, Zn, Cd, Si, Ti, Zr, Th, Pb, Al, As, Sb, totalling not more than 20 wt%. Combinations are covered in 15 claims.

Author
Pilkington Bros Ltd
Origin
Unknown
Journal Title
Usp 3 029 152, 10/4/62
Sector