With limited competition and few high-grade resources worldwide, the market for high-purity quartz should be a tough nut to crack. However, with leading producers working side-by-side and others focusing on targeted end-market specifications, progress has been steady even throughout the challenging financial period of late. This article takes a closer look at these projects.