High-Pull Forehearths Meet High Expectations

With the current focus on glass manufacturing in Mexico, this article provides a case study on the introduction of high-pull foreherarths at a plant in the state of Queretaro, Mexico. An overview of the cooling concept involved also highlights how the forehearth design is aimed at reaching high efficiency in thermal homogeneity.