High Performance Glass For Demanding Architecture

The Stockholm Victoria Tower project was an award winner in the hotel/leisure class at the World Architecture Festival in Singapore in 2012. This article describes the project. The facade is a composition of 10,000 square/m of reflecting, triangular IG units in shades of gold, bronze and silver. Manufacturer of this high-tech curtain walling glass was AS Klaasimeister, Estonia's leading flat glass producer.