High Index Optical Glass

Has high refractive index and low absorption in the visible, and contains TeO2, La2O3, B2O3, K2O, Ta2O5 and GeO2.

Author
Eatsman Kodak Co
Origin
Unknown
Journal Title
Usp 3 690 908, 12/9/72
Sector
Refractive Indexes
Class
RI 35

Request article (free for British Glass members)

High Index Optical Glass
Usp 3 690 908, 12/9/72
RI 35